Interlocking concrete paver blocks are widely used for pedestrian and light-to-medium vehicular pavements, but their cement content carries a high environmental cost. This study investigates M40-grade, 80 mm thick, I-shaped paver blocks (200 × 160 mm in plan) made with nylon fibre, fly ash (FA) and rice husk ash (RHA). In the first phase, nylon fibre was added at 0.1–0.5% by weight of cement to identify the optimum dosage. In the second phase the optimum dosage (0.3%) was held constant while ordinary Portland cement (OPC) was replaced by 10, 20 and 30% FA or RHA. Slump, apparent and corrected compressive strength (IS 15658:2021) and flexural strength were measured at 7, 14 and 28 days. The 0.3% fibre mix gave the highest strength among the fibre-only mixes (44.26 N/mm² at 28 days, +4.8% over the control value of 42.24 N/mm²), whereas dosages of 0.1, 0.2, 0.4 and 0.5% fell below the control. With 0.3% fibre, 20% FA gave 44.89 N/mm² (+6.3%) and 10% RHA gave 48.70 N/mm² (+15.3%; corrected strength 57.5 N/mm²); 30% replacement of either material reduced 28-day strength below the control. Flexural strength followed the same ranking, reaching 5.09 N/mm² (20% FA) and 5.31 N/mm² (10% RHA) against 4.94 N/mm² for the control. Slump decreased with fibre (83 mm to 71 mm at 0.5%) and with RHA (down to 58 mm at 30%) but increased with FA (up to 110 mm). The mean corrected 28-day strength of every mix exceeded the 40 N/mm² requirement of M40 grade. The results indicate that 20% FA or 10% RHA combined with 0.3% nylon fibre allows a 10–20% reduction in OPC without loss of strength. Abrasion resistance, water absorption and long-term durability were not evaluated and must be verified before field use.

Other Details

Paper ID: IJSRDV14I90083
Published in: Volume : 14, Issue : 9
Publication Date: 01/12/2026
Page(s): 176-181

Article Preview

Download Article